There is no universal hardness conversion formula: steel conversions use ASTM E140/SAE J417 reference data and linear interpolation between published anchor points.
A request for a hardness conversion formula often assumes that HRC, HRB, Vickers and Brinell are interchangeable units. They are not. Each test uses a different indenter and load, so each produces a numerical value based on a different measurement method. For suitable steels, an empirical conversion table is the practical method for estimating the equivalent value on another scale.

What the hardness conversion formula actually represents
Hardness conversion tables are built by measuring the same steel specimens with different testing methods and pairing the results. Those paired values become anchor points in a published reference table. A calculator can then return the tabulated value when the input lands on an anchor or estimate a value between anchors.
The underlying lookup-and-interpolation method can be expressed as:
Converted value = y1 + ((x − x1) ÷ (x2 − x1)) × (y2 − y1)
In this expression, x is the measured input hardness, while x1 and x2 are the neighboring anchor values on the input scale. The values y1 and y2 are their corresponding values on the scale being calculated. This is a linear-interpolation formula, not a universal physical law for every metal or hardness test.
The Hardness Conversion Calculator applies this table-based method automatically. Enter one known steel hardness value and it updates the equivalent Rockwell, Vickers and Brinell values, together with an approximate ultimate tensile strength in MPa and ksi.
Choose the scale that matches your test
Start with the scale printed on the test report or shown by the instrument. Choosing a scale based on the answer you want rather than the measurement you already have can produce an unsupported result.
| Scale | Indenter and load | Typical use and stated range |
|---|---|---|
| Rockwell C (HRC) | Diamond cone under a 150 kgf load | Hardened steels, roughly HRC 20 to 68 |
| Rockwell B (HRB) | 1/16-inch steel ball under a 100 kgf load | Softer steels, up to about HRB 100 |
| Vickers (HV) | Diamond pyramid | Defined across the whole range, making it a useful conversion-table backbone |
| Brinell (HB) | 10 mm ball under a 3000 kgf load | About HB 100 to 650; above roughly HB 650, a tungsten-carbide-ball Brinell test is designated HBW |
Rockwell C and Rockwell B have very little overlap. HRC is intended for harder steel, while HRB covers the softer end of the steel range. A hardness that is too soft for HRC or too hard for HRB is not converted into a misleading number. Instead, the appropriate Rockwell result is marked “not defined.”
Vickers values span the full range, but that does not make every conversion equally applicable. The material still has to fall within the steel family for which the table was calibrated. The same caution applies to Brinell: its ball diameter, test load and ball material are part of the test definition.
Convert a steel hardness value
- Open the Hardness Conversion Calculator and choose the scale you already know: Rockwell C (HRC), Rockwell B (HRB), Vickers (HV) or Brinell (HB).
- Type the measured hardness value in the selected field. Check the table range displayed beneath the field before continuing.
- Read the equivalent values as the number changes. Rockwell, Vickers, Brinell and approximate tensile-strength results update while you type; there is no button to press.
- Review every output label. An “out of range” message means the entered value lies beyond the available table, while “not defined” means that the selected equivalent scale does not apply at that hardness.
No file or other material needs to be uploaded, and nothing is sent with the entered number. The workflow is therefore quick and private, but the material and scale checks still matter because automation cannot repair an invalid conversion assumption.
How anchors, interpolation and range checks work
An anchor point is a hardness value explicitly listed in the published conversion table. When the input equals an anchor, the calculator returns that standard tabulated number. For a value between two anchors, it estimates the result by linear interpolation using the formula shown earlier.
Interpolation is useful because it fills gaps between listed values without pretending that the relationship continues indefinitely. It also does not remove the uncertainty inherent in comparing different tests. The estimate reflects the straight-line relationship between neighboring table rows, while the underlying hardness relationship remains empirical.
The range controls are equally important. If an input falls beyond the end of a scale’s table range, the calculator reports it as out of range rather than extrapolating a made-up result. A “not defined” response is different: it indicates that the equivalent scale has no valid application at that hardness. This can occur because Rockwell C is undefined for very soft steel and Rockwell B saturates near HRB 100.
These two messages help distinguish a missing table value from an inapplicable test scale. In engineering work, that distinction should be retained in any record, report or follow-up calculation rather than replacing either status with a guessed number.
An exact-anchor steel example
Suppose a steel test report gives HRC 20. Enter 20 with Rockwell C selected. Because HRC 20 is a published anchor, the lookup returns HV 238, HB 222 and HRB 97 without estimating between rows.
Read the result as HRC 20 being approximately equivalent to HV 238, HB 222 and HRB 97 for the material covered by the table. The calculator also updates its approximate tensile-strength estimate in MPa and ksi. Those converted numbers do not change the original test method or prove that all four scales would produce identical readings on every steel.
Interpret converted values and tensile strength correctly
A converted hardness value is an estimate of how the same material is expected to appear under a different test method. It should retain the same units and scale designation as the corresponding output. A value such as HB 654, for example, means an approximate Brinell-equivalent result for a compatible steel; it does not mean that a Brinell indenter was used.
The approximate ultimate tensile-strength output is included because, for carbon and low-alloy steel, ultimate strength tracks hardness closely enough to provide a useful estimate. The figure is drawn from the same ASTM E140-based conversion data, so it should be treated as a guide in MPa or ksi rather than as independently measured material data.
Do not use the tensile estimate as a substitute for a real tensile test, especially for critical or safety-related parts. If the design requires a certified strength value, specimen information, or proof of compliance, obtain that through the appropriate testing and documentation process.
Material limits that affect conversion accuracy
This calculator is calibrated for non-austenitic carbon and low-alloy steels. Austenitic stainless steel, tool steel, hardened surfaces, cast iron and non-ferrous metals such as aluminum, copper and brass follow different hardness relationships. A converted value for those materials can differ substantially from the value obtained by the appropriate direct test.
Material identity is therefore part of the calculation, even though the input field contains only a hardness number. Confirm that the component belongs to the calibrated material category before relying on a result. When accuracy matters, test the actual part on the required scale instead of treating a converted figure as a substitute for measurement.
The word “steel” also needs a suitable definition here. It describes the non-austenitic carbon and low-alloy family covered by the reference data, not every metal containing iron. The tool’s broad label should not be used to extend ASTM E140-based relationships to an unrelated alloy family.
A practical verification routine
- Confirm the material: Check that the component is within the non-austenitic carbon and low-alloy steel range covered by the table.
- Confirm the source scale: Match the input to the test report, including the Rockwell subtype—HRC or HRB—and the scale’s units.
- Check the displayed range: Keep the entered value inside the range shown beneath the input field.
- Preserve status messages: Record “out of range” or “not defined” rather than silently substituting a nearby value.
- Cross-check the reading: For a side-by-side reference while reviewing a result, see the Hardness Conversion Chart for Steel: HRC, HRB, HV & HB guide.
- Classify the result correctly: Treat converted hardness as an empirical estimate and the tensile-strength figure as a rough guide, not a substitute for a direct test.
If you're weighing options, Curved Surface Area of Hemisphere: Accurate Formula covers this in detail.